Fig. 6

XRD patterns of as-received HAp powder (a), as-received β-TCP powder (b), and (c) the sintered 3D-printed bioceramic scaffolds sintered at 1150 °C for 2h
XRD patterns of as-received HAp powder (a), as-received β-TCP powder (b), and (c) the sintered 3D-printed bioceramic scaffolds sintered at 1150 °C for 2h