Table 1 Characterization of molar ratio and ions percentage (Mg/Ca) within HA-based nanoparticles by ICP-AES, crystallinity degree by XRD, and the organic content by thermogravimetric analyses

From: Chitosan biomineralized with ions-doped nano-hydroxyapatite tunes osteoblasts metabolism and DNA damage

Sample

Ca/P

[Mg (or Fe) + Ca]/P

Mg (%)

Fe (%)

Crystallinity degree (%)

Organic content (w/w %)

MgHA/CH

1.61

1.70

6

/

8

33

MgHA

1.56

1.61

3

/

12

/

FeHA/CH

1.34

1.67

1

24

/

22

FeHA

1.23

1.62

1

31

/

/