Skip to main content

Table 1 Composition (wt%), liquid-to-powder ratio (L/P), and setting time (Ts) of the Ca-Si-Li cement

From: Lithium-doped calcium silicate cement regulates the immune microenvironment and promotes M2 macrophage polarization for enhancing bone regeneration

Code

CaO

SiO2

Al2O3

LiO

L/P (mL/g)

Ts (min)

Li0

65

30

5

0

0.35

16.0 ± 1.7

Li5

60

30

5

5

0.33

14.6 ± 1.9

Li10

55

30

5

10

0.32

11.9 ± 2.2