Skip to main content
Fig. 3 | Journal of Biological Engineering

Fig. 3

From: The stability and self-assembly of tri-calcium silicate and hydroxyapatite scaffolds in bone tissue engineering applications

Fig. 3

Analyzing the integration of TCS in SA hydrogel through Rg, RMSF, and H-bond (A) TCS molecules (purple) in the SA hydrogel (yellow), containing the water molecules (blue), showed the increasing of TCS content from 0 to 40 wt% in composition; (B) Rg analysis; (C) RMSF analysis; and (D) averaged normalized H-bond with water analysis. All the analyses confirmed that 10 wt% TCS has the best and optimal state over the simulation

Back to article page